http://www.w3.org/ns/prov#value
  • In one embodiment, the absorbing material loading level can range from 10% to 20%, 20% to 40% and 40% to 60% by weight with respect to the polymer.In another embodiment, for example, the composition of the present invention may include a desiccant such as molecular sieves (i.e. component C), polypropylene (i.e. component A) and polyglycol (i.e. component B).
http://www.w3.org/ns/prov#wasQuotedFrom
  • patentgenius.com