| http://www.w3.org/ns/prov#value | - In these experiments, described particularly in relation to Figure 3, samples were solution treated at 575 C for 24. hours, water quenched, and then reheated and held at temperatures separated by steps of 50 C between 300 and 450 C. The microstructures produced from the tests carried out on full scale ingots are shown in Photo 2.
|