  • When the water-soluble polymer is compounded in the polishing slurry of the present invention, the amount of the water-soluble polymer to be compounded is preferably 0.001 to 10 g, more preferably 0.01 to 2 g and particularly preferably 0.1 to 1 g based on the polishing slurry of 100 g in gross weight.