  • After a preliminary reaction time of about 10 minutes, the lacquer mixture is applied to a support and coating films are obtained which have the following properties: Drying time minutes Pendulum hardness according to Albert Konig (DIN 53,157) after 10 days sec 118 Erichsen-depression (DIN 53,156) mm 7.7 The films are resistant to solvents such as xylene, tolulene, butyl acetate or ethyl acetate.