| http://www.w3.org/ns/prov#value | - As shown in FIG. 2B, the re-distribution technology is accomplished by first using an electrically conductive material such as aluminum or copper to form a trace 217 on a power pad 213 that is partly exposed to outside of a passive film 218 and all the traces 217 on the power pad 21 are consolidated to form the power plane 21.
|