| http://www.w3.org/ns/prov#value | - A method of preparing a silicate-based yellow phosphor having the formula A2SiO4:Eu2+D, wherein A is at least one of a divalent metal selected from the group consisting of Sr, Ca, Ba, Mg, Zn, and Cd; and D is a dopant selected from the group consisting of F, Cl, Br,and I, wherein D is present in the phosphor in an amount ranging from about 0.01 to 20 mole percent, the method comprising using a wet
|