| http://www.w3.org/ns/prov#value | - (i) the coating of glass or plastic beads must be scraped onto a surface free of dust, including a clean weighing paper or pan, using a clean stainless steel razor blade or other clean sharp instrument that will not contaminate the sample with lead.
|