| http://www.w3.org/ns/prov#value | - A resin for forming a layer 32 is dissolved in a volatile solvent including alcohols such as methanol and ethanol, ketones such as methyl ethyl ketone and acetone, and the resultant coating liquid is applied onto a transparent base film 31 by a method such as bar coating, dipping, spraying and spin coating, and dried.
|