  • r asphalt-solvent to saturate the entire aggregate; adding rubber to the saturated aggregate so the finished mixture contains only /2 of one percent rubber based on the weight of the total asphalt added; adding asphalt or other bituminous material to the mixture at a temperature of 250F or higher.