  • According to one embodiment, the barrier layer is formed of a mixture of ethylene-vinyl acetate copolymer (EVA) and polypropylene (PP), preferably comprising about 5% to about 35% PP, more preferably about 10% to about 30% PP, more especially preferably about 15% to about 25% PP, and most preferably about 20% PP, with the balance comprising ethylene-vinyl acetate (E