http://www.w3.org/ns/prov#value | - The substrate is then heated at 325??? C. for approximately 24 hours or other suitable time to allow by-products of nanofiber polymer decomposition to diffuse out, forming a nanochannel from the depolymerized nanofiber, which effectively acts as a sacrificial layer.
|