| http://www.w3.org/ns/prov#value | - First, as diagrammed in FIG. 11(A), a metal layer. 3220 is built up on a transparent substrate 310, to a film thickness of 0.1 to 0.5??, by a dry plating process such as sputtering, vapor deposition, or chemical vapor deposition, for example.
|