  • However, a polymer obtained by for example bulk polymerization, suspension polymerization or solution polymerization is heat-treated generally at 60???-250??? C., or preferably at 80???-200??? C. In this case, when the polymer is obtained by the solution polymerization method, its heat treatment may be carried out concurrently with its drying or with the evaporation of the solvent.