http://www.w3.org/ns/prov#value | - The coatings according to the invention can be produced by known methods, for example, by spraying, application by a doctor blade, dipping, application with roller applicator systems, by printing processes such as gravure printing, silk screen printing, curtain casting, and can be dried at room temperature or at temperatures of up to 300??? C., preferably up to 200??? C.
|