PropertyValue
http://www.w3.org/1999/02/22-rdf-syntax-ns#type
http://www.w3.org/ns/prov#value
  • When the polymer is a thermoplastic elastomer, preferably the amount of thermoplastic elastomer used to prepare the aqueous emulsion is between about 2% and about 10%, and more preferably between about 5% and about 10%, by weight of the aqueous emulsion.
http://www.w3.org/ns/prov#wasQuotedFrom
  • google.com