| http://www.w3.org/ns/prov#value | - The agents according to the invention are advantageously applied from an aqueous bath and are advantageously employed therein in such an amount that for every 1 g of polyamide there is available 5 to 800 ??g, in particular 10 to 200 ??g, of copper metal.
|