| http://www.w3.org/ns/prov#value | - Then, substrate 21 is put into a sputtering reaction chamber (not shown), in which a first metal layer 27 is formed by depositing a metal such as aluminum (Al) or Al alloy, at a temperature of 150??? C. or less and under a predetermined degree of vacuum.
|