PropertyValue
http://www.w3.org/1999/02/22-rdf-syntax-ns#type
http://www.w3.org/ns/prov#value
  • According to the present invention, a zeolite, preferably a ZSM-5 zeolite, and the binder can be well mixed by any means known to one skilled in the art such as stirring, blending, kneading, or extrusion, following which the zeolite-binder mixture can be dried in air at a temperature in the range of from about 20 to about 800??? C., for about 0.5 to about 50 hours under any pressures that accommod
http://www.w3.org/ns/prov#wasQuotedFrom
  • google.es