  • The reaction can be carried out in a suitable solvent by addition of G-M to a dry solution of the polybenzoxazole precursor base polymer at a temperature from about ???25??? C. to about 40??? C. The more preferred temperature is from about 0??? C. to about 25??? C. The most preferred temperature is from about 5??? C. to about 10??? C. The reaction time is from about 1 hour to about 24 hours.