| http://www.w3.org/ns/prov#value | - According to, for example, Japanese Patent Application (Kokai) Nos. 7-130652 and 8-78329, a crystalline silicon film is obtained by the heat treatment conducted at 550??? C. for 4 hours by introducing such a metal element as nickel into the amorphous silicon film.
|