| http://www.w3.org/ns/prov#value | - FIG. 7 is a graph of 28-day dry compressive strength of cementitious mixtures as a function of weight ratio of calcined gypsum to OPC (and with a constant ratio of metakaolin to OPC), in which the narrow range of optimal, high-compressive strength mixtures of the present invention is demonstrated.
|