| http://www.w3.org/ns/prov#value | - The electrode group is pressurized under a high temperature of 30??? C. or higher and under a reduced pressure including vacuum or atmospheric pressure with a pressure falling within a range of between 0.05 kg/cm2 and 10 kg/cm2 to allow the electrode group to have a predetermined thickness, thereby forming an electrode group.
|