| http://www.w3.org/ns/prov#value | - However, when the degradable strands 9, 11 or tapes 25 aredegraded at selected regions along its length (in any known or other manner), this will affect the stiffness and flexibility of the carrier throughout its length (and hence of the extrusion, e.g. edge trim, in which it is located) significantly.
|