  • Sidewall spacers 312 can be formed by blanket depositing a conformal insulating film, such as silicon nitride, silicon oxynitride, or silicon oxide or a combination thereof over substrate 300 and gate electrode 310 and then anisotropically etching back the dielectric film to form spacers 312.