| http://www.w3.org/ns/prov#value | - ed by depositing a layer of phase change material on the structure illustrated in FIGS. 12A-12D, etching back the phase change material using for example Reactive Ion Etching to form elements 160, and forming bit line material and performing a planarization process such as CMP to form the bit lines 120.
|