  • After the reactor was thoroughly purged with nitrogen to remove any catalyst poisons, such as moisture and oxygen, 10 mg of solid pro-catalyst component were charged into the reactor as a 1 weight percent mixture in dry mineral oil, followed by addition of triethylaluminum co-catalyst in a prescribed amount to obtain an Al/Ti molar ratio of about 200:1. 300 g of liquid propylene were then charged