  • The ferromagnetic coupling layer 306 and 356 may have a thickness of approximately 0.2 nm to 10 nm and may comprise, for example, Ru, Au, Mn, Os, Ir, Rh, Cu, Cr, a CoRu alloy or a CoRu alloy doped with B, Ru and Cr, a CoCr alloy, Pt, or Pd or any other alloys or other combinations of the above materials.