| http://www.w3.org/ns/prov#value | - The reason is that lanthanum chromite doped with an element other than Ca requires firing at a temperature higher than 1500??? C. for fabricating a membrane free of gas permeability, and if the solid oxide fuel cell is fired at this temperature, reactions take place between other constituting materials, and the output performance is deteriorated.
|