PropertyValue
http://www.w3.org/1999/02/22-rdf-syntax-ns#type
http://www.w3.org/ns/prov#value
  • he photoresist film 9 is removed and thereafter, a device separation groove 5 is formed by polishing the silicon oxide film 7 by the CMP method using the silicon nitride films 3 and 8 as stoppers and leaving the film 7 in the groove 5a.Then, the silicon nitride films 3 and 8 are removed by the wet etching using hot phosphoric acid and thereafter, ions of an n-type impurity such as P (phosphorus) a
http://www.w3.org/ns/prov#wasQuotedFrom
  • patentgenius.com